Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 |
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Bent Strip, Compression Molded; ASTM D1693 |
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L43840U Rotational Molding LLDPE
(discontinued **) Butene CopolymerApplications: Toys and other non-tank rotational molding applications.Formolene L43840U is a Butene Copolymer of linear low density polyethylene for toys and other non-tank rotationa.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L63550U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63550 is fully heat and UV stabilized.Meets all requirements.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 |
NIZHNEKAMSKNEFTEKHIM PE 6844G (446H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Environmental Stress Crack Resistance | 1000 hour | 1000 hour | |
NOVA Chemicals Sclair® 35BP HDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F0, ASTM D1693 |
NOVA Chemicals Sclair® 96A-UV8D HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, superior strength, gel free, excellent UV resistance.Applications: Oriented tapes for industrial woven bags and tarpaulins, monoaxial or.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 |
ExxonMobil HD 9856BA Blow Molding Resin
(discontinued **) HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracki.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Novapol® TR-0338-U MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LP5002 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LP series of polyethylene resins exhibits excellent environmental stress crack resistance and is especially designed for bottles containing aggressive agricultural and hou.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition A - 10% Igepal®; ASTM D1693 |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
Environmental Stress Crack Resistance | 1000 hour | 1000 hour | ASTM D1693 |
Global B-8200 High Density Polyethylene Description-high molecular weight, excellent stress cracking resistance,
excellent impact strength to blow moldApplications-large drums, gasoline tanks, agricultural chemical tanksInformation provi.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 |
Micropol Microlink XL Crosslinkable Polyethylene Characteristics: exceptional toughness, exceptional enviromental stress cracking resistance, outstanding low temperature impact resistance down to -40°C, fully stabilized for outdoor use world wi.. |
|||
Environmental Stress Crack Resistance | 1000 hour | 1000 hour | |
JPJ Technologies 6360M HDPE Extrusion Information provided by JPJ Technologies |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Molded; F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene ApplicationsPETROTHENE LP 5402-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good draw-down. LP 5402-0.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition B, 100% Igepal, F50; ASTM D1693 |
Ineos K44-06-122 HDPE HDPE K44-06-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as .. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded, 10% Igepal; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded, 10% Igepal; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties with.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded, 10% Igepal; ASTM D1693 |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1693 |
SCG Chemicals EL-Leneâ„¢ H5604F High Density Polyethylene Film Key Characteristics:High tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierRecommended Applications: Films for shopping bag, T-shirt bag, garbage bag, liner bagInfor.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1639 |
SCG Chemicals EL-Leneâ„¢ L1810F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesContains 1600 ppm slip agent and 1900 ppm antiblocking agentRecommended Applications:Film for heavy duty bag, industrial bag, rice bag, su.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | No failures; ASTM D1693 cond. C 100% lgepal |
Total HP 401N Natural HDPE, pipe Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | SP-NCTL; ASTM D5397 |
Formosa Plastics Formolene® HL3812 Film (Hexene) HDPE Medium Density Polyethylene Formolene® HL3812 is a high molecular weight hexene copolymer resin that is tailored specifically for geomembrane applications. The resin provides an excellent balance o.. |
|||
Environmental Stress Crack Resistance | 1000 hour | 1000 hour | F50; ASTM D1693 |
UBE UMERIT 1520F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F50, Anatrox 100%; ASTM D1693B |
Total Lumicene® mPE M 3509 Medium Density Polyethylene, Blow Molding Lumicene® mPE M 3509 is a metallocene-based medium density polyethylene combining the features of conventional blow molding polyethylene with differentiated optical propertied such as gloss and co.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature >=50.0 °C |
>= 1000 hour @Temperature >=122 °F |
Igepal (no failures); ASTM F1248 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F0, ASTM D1693 |
NOVA Chemicals Sclair® 94D1 HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, high stretchability, excellent strength.Applications: Package nettings for produce, Christmas tree wrap and turkey overwrap.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | 1000 - 5000 hour | 1000 - 5000 hour | Average value: 2290 hour Grade Count:10 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 2915 HDPE Injection Molding Resin
(discontinued **) Features: Excellent balance of stiffness and toughness, low odor, permits light weight container design.Applications: Thin walled food containers, frozen food containers.Data provided by the manufac.. |