Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F130-C PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F130-C2 PA6 Medium Viscosity, Film Extrusion, Lubricated |
|||
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F130-C3 PA6 Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated |
|||
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F132 PA6 Film Extrusion, High Viscosity |
|||
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F132-C1 PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F234-C PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., Film; DIS 15105-1/-2 |
DSM Akulon® XP36-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., film; DIS 15105-1/-2 |
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |
|||
Oxygen Transmission | 1.30 cc-mm/m²-24hr-atm @Temperature 23.0 °C |
3.30 cc-mil/100 in²-24hr-atm @Temperature 73.4 °F |
at 0% r.h., Film; DIS 15105-1/-2 |
DSM Akulon® XP32-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |