Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 67.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
170 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
670 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2665 MAS071 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Oxygen Transmission | 67.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
170 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
670 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
Oxygen Transmission | 67.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
170 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
670 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Oxygen Transmission | 67.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
170 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
670 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Oxygen Transmission | 67.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
170 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
670 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Oxygen Transmission | 67.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
170 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
670 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® LQ2647 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g.. |