Polymer Property : Oxygen Transmission = 1.30 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., film; DIS 15105-1/-2
DSM Akulon® F127 PA6
Low/Medium Viscosity, Film Extrusion
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., film; DIS 15105-1/-2
DSM Akulon® F130 PA6
Film Extrusion, Medium Viscosity
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., film; DIS 15105-1/-2
DSM Akulon® F130-C PA6
Film Extrusion, Medium Viscosity, Lubricated
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., film; DIS 15105-1/-2
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., film; DIS 15105-1/-2
DSM Akulon® F130-C3 PA6
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., film; DIS 15105-1/-2
DSM Akulon® F132 PA6
Film Extrusion, High Viscosity
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., film; DIS 15105-1/-2
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., film; DIS 15105-1/-2
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., Film; DIS 15105-1/-2
DSM Akulon® XP36-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., film; DIS 15105-1/-2
DSM Akulon® F128 PA6
Film Extrusion, Medium Viscosity
Oxygen Transmission 1.30 cc-mm/m²-24hr-atm

@Temperature 23.0 °C
3.30 cc-mil/100 in²-24hr-atm

@Temperature 73.4 °F
at 0% r.h., Film; DIS 15105-1/-2
DSM Akulon® XP32-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated