Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.190 - 3.60 cc-mm/m²-24hr-atm | 0.483 - 9.14 cc-mil/100 in²-24hr-atm | Average value: 1.15 cc-mm/m²-24hr-atm Grade Count:7 |
Overview of materials for Nylon 66, Film This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat.. |