Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 15.4 cc-mm/m²-24hr-atm @Temperature 25.0 °C |
39.1 cc-mil/100 in²-24hr-atm @Temperature 77.0 °F |
ASTM D1434 |
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating Parylene N, poly(para-xylylene), is a completely linear, highly crystalline material. Parylene N is a primary dielectric, exhibiting a very low dissipation factor, high dielectric strength, and a lo.. |