Polymer Property : Oxygen Transmission = 376 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 148 cc-mm/m²-24hr-atm
376 cc-mil/100 in²-24hr-atm
or 7800 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Clysar® HP Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, linear low-density polyolefin film. Cross-linking produces a film that is extremely rugged and durab..
Oxygen Transmission 148 cc-mm/m²-24hr-atm
376 cc-mil/100 in²-24hr-atm
or 7800 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Clysar® LLP Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, nonirradiated, heat-shrinkable, linear low-density polyolefin film. LLPS is the silicon treated, hot slip version of ..