Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission 132 cc-mm/m²-24hr-atm
335 cc-mil/100 in²-24hr-atm
or 2600 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® LWS-1 LMDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one..
Oxygen Transmission 132 cc-mm/m²-24hr-atm
335 cc-mil/100 in²-24hr-atm
or 2600 cc/m²-24hr-atm for the film. ASTM D3985
DuPont™ Sclairfilm® LWS-2 LMDPE Film, Laminating, 50.8 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.LWS is a linear medium density polyolefin film produced from Sclair® copolymer resin and designed primarily for laminating end uses. It is treated on one..