Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.590 cc-mm/m²-24hr-atm | 1.50 cc-mil/100 in²-24hr-atm | or 39 cc/m²-24hr-atm for the film at 23°C, 0% RH. ASTM D1434-66 |
DuPont™ Dartek® O-401 Nylon 6,6 Oriented Film, 15 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A machine direction oriented nylon type 6,6 film. Many of the properties of nylon 6,6 film are improved upon orientation, but particularly the overall tou.. |
|||
Oxygen Transmission | 0.590 cc-mm/m²-24hr-atm | 1.50 cc-mil/100 in²-24hr-atm | or 39 cc/m²-24hr-atm for the film at 23°C, 0% RH. ASTM D1434-66 |
DuPont™ Dartek® UF-410 Nylon 6,6 Oriented Film, 15 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A monoaxially oriented nylon 6,6 film with good "slip" characteristics, which ensure excellent machinability/runnability even at high relative humidity con.. |