Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.0300 cc-mm/m²-24hr-atm | 0.0762 cc-mil/100 in²-24hr-atm | 20°C- 65% RH; based on 20 µm layer |
Noltex Soarnol® A4412 Ethylene Vinyl Alcohol Copolymer Ethylene content 44 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Oxygen Transmission | 0.0300 cc-mm/m²-24hr-atm | 0.0762 cc-mil/100 in²-24hr-atm | 20°C- 65% RH; based on 20 µm layer |
Noltex Soarnol® AT4403 Ethylene Vinyl Alcohol Copolymer High ethylene content, low melting point. Suitable for use in multilayer structures where ease of thermoforming is required. Ethylene content 44 mol%.The gas barrier property of Soarnol is about fo.. |
|||
Oxygen Transmission | 0.0300 cc-mm/m²-24hr-atm | 0.0762 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
Oxygen Transmission | 0.0300 cc-mm/m²-24hr-atm | 0.0762 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Oxygen Transmission | 0.0300 cc-mm/m²-24hr-atm | 0.0762 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr.. |