Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 7.00 cc-mm/m²-24hr-atm | 17.8 cc-mil/100 in²-24hr-atm | ASTM D3985 |
Eastman Cadence™ GS1 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |