Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 225 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
572 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
Based on 1 mil (0.0254 mm) thick film; ASTM D3985 |
DuPont Elvax® 3130SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |
|||
Oxygen Transmission | 225 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
572 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
Based on 1 mil (0.0254 mm) thick film; ASTM D3985 |
DuPont Elvax® 3130SBZ Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
(discontinued **) 12 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra.. |