Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 2.76 cc-mm/m²-24hr-atm | 7.01 cc-mil/100 in²-24hr-atm | Tested per ASTM D3985 at 22°C |
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL13 (formerly known as XM110) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat seal.. |
|||
Oxygen Transmission | 2.76 cc-mm/m²-24hr-atm | 7.01 cc-mil/100 in²-24hr-atm | Tested per ASTM D3985 at 22°C |
DuPont Teijin Films Mylar® RL4 Polyester Packaging Film, 75 Gauge Data provided by DuPont Packaging Polymers.Mylar® RL4 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film .. |