Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 198 cc-mm/m²-24hr-atm | 503 cc-mil/100 in²-24hr-atm | or 3900 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Oxygen Transmission | 198 cc-mm/m²-24hr-atm | 503 cc-mil/100 in²-24hr-atm | or 3900 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Oxygen Transmission | 198 cc-mm/m²-24hr-atm | 503 cc-mil/100 in²-24hr-atm | or 3900 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Oxygen Transmission | 198 cc-mm/m²-24hr-atm | 503 cc-mil/100 in²-24hr-atm | or 3900 cc/m²-24hr-atm for the film. ASTM D3985 |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |