Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 2060S (60105) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4020R (20405) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 3.0 - 6.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
3.0 - 6.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 20; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4148B (484H2) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4430S (30405) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4435S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4431S (30405) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4436S (35405) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 3.5 - 6.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 - 6.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3501 SHF Description: Super High FlowInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 - 6.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Breplast Bretene SPF Thermoplastic Composite, 40% PP + 60% PE Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |