Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.5 - 2.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.5 - 2.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Lushan L-5R (F) Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |