Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.0 - 11 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.0 - 11 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Polymer Resources ABS-GP-IM General Purpose ABS, Impact Modified General Purpose Acrylonitrile Butadiene Styrene, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Melt Flow | 5.5 - 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 - 11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Melt Flow | 5.5 - 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 - 11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |