Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.6 g/10 min @Load 5.00 kg, Temperature 280 °C |
7.6 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Melt Flow | 7.6 g/10 min @Load 5.00 kg, Temperature 300 °C |
7.6 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |