Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.2 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.2 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
SABIC Innovative Plastics Geloy XTWE265 ASA Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 5.2 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.2 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
SABIC Innovative Plastics Geloy XTWE265 ASA (Europe-Africa-Middle East) Highly weatherable Geloy ASA profile extrusion grade for processes with simple or no calibration hardware.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 5.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 5.2 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.2 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM-D1238, ISO 1133 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Melt Flow | 5.2 g/10 min @Load 6.60 kg, Temperature 337 °C |
5.2 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Melt Flow | 5.2 g/10 min @Load 5.00 kg, Temperature 265 °C |
5.2 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
Diamond Polymers ABSPC 9901B ABS/PC Blow Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 5.2 g/10 min @Load 5.00 kg, Temperature 265 °C |
5.2 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
Diamond Polymers ABSPC 9901B-50148 ABS/PC Blow Molding Grade, High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 5.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-765 ABS - Flame Retardant F.R. High Flow |
|||
Melt Flow | 5.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |
|||
Melt Flow | 5.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET
(Unverified Data**) Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various.. |