Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® FR30U ABS Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 260 °C |
28 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East) UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 28 g/10 min @Load 3.80 kg, Temperature 230 °C |
28 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 (I) |
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Kingfa FRABS-518 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmLow temperature impact resistanceApplications:Injection moldingPower tools accessoriesInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 190 °C |
28 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) I2 HB 7250 High Density Polyethylene I2 (HB 7250) is a high density polyethylene with Propylene as comonomer. It is easy flowing, low warpage, less hard and stiff than I1.Applications: household articles, closures/seals, packaging.Info.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 360 °C |
28 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 360 °C |
28 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 360 °C |
28 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 360 °C |
28 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Asia Pacific) Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 360 °C |
28 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 265 °C |
28 g/10 min @Load 11.0 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® X6125 PBT+PC Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 285 °C |
28 g/10 min @Load 4.76 lb, Temperature 545 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/PBT IM 1012 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Melt Flow | 28 g/10 min @Load 2.16 kg, Temperature 285 °C |
28 g/10 min @Load 4.76 lb, Temperature 545 °F |
ASTM D1238 |
Techmer ES Plastiblend® PC/PET IM 1016 UV Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238; ISO 1133 |
Styron MAGNUMâ„¢ 8391 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 8391 ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Melt Flow | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238; ISO 1133 |
Styron Magnumâ„¢ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ MED ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass (continuous process) ABS technology of Styron ensures an ABS resin that .. |
|||
Melt Flow | 28 g/10 min @Load 5.00 kg, Temperature 360 °C |
28 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Melt Flow | 28 g/10 min @Load 21.6 kg, Temperature 190 °C |
28 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis BS2581 High Density Polyethylene for Blow Molding BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, househol.. |
|||
Melt Flow | 28 g/10 min @Load 21.6 kg, Temperature 190 °C |
28 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GF4950 HDPE Blow Molding Polyethylene Copolymer HDPE GF4950 is a high-density polyethylene copolymer with well balanced properties between impact and stiffness combined with high environmental stress cracking resistance and processability. It was.. |
|||
Melt Flow | 28 g/10 min @Load 21.6 kg, Temperature 190 °C |
28 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GF4960 HDPE Blow Molding Polyethylene Homopolymer GF 4960 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance. It was developed for the blow-molding segment. It is used in containers for y.. |
|||
Melt Flow | 28 g/10 min @Load 21.6 kg, Temperature 190 °C |
28 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Braskem Green PE SGF4950 Blow Molding and Monofilament High Density Polyethylene Description: SGF4950 is a high-density polyethylene copolymer, developed for the blow-molding segment. It shows well balanced properties between impact and stiffness, combined with high environmenta.. |
|||
Melt Flow | 28 g/10 min @Load 8.70 kg, Temperature 190 °C |
28 g/10 min @Load 19.2 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Elastamax HTE 2101-1000 Polyurethane Alloy
(discontinued **) This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. .. |
|||
Melt Flow | 28 g/10 min @Load 21.6 kg, Temperature 190 °C |
28 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene Description: SGF4960 is a homopolymer high-density polyethylene, developed for the blow-molding segment with high density and stiffness combined with high impact resistance. The minimum biobased con.. |