Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers SAN 278 Medium Blue Tint Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers SAN 279 Water White Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers Softflex® 7200 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
2.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Melt Flow | 2.0 - 4.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
2.0 - 4.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio < 20; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4252A (524H1) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 2.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
2.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
EVALCA EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applicat.. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kingfa FW-650 Flame Retardant ABS Features:Weather resistanceSuper high impact resistanceApplications:Injection moldingSwitchSocketInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kingfa H-12 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh toughnessHeat resistanceApplications:Automobile exterior trimAutomobile interior trimPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Imerys ImerPlastâ„¢ 10WPCT Recycled Polyolefin Resin A black, UV stabilized, recycled resin with no significant odor, for compounding with wood flour for extruded decking applications. With added reinforcing filler and wood flour dispersant, ImerPlast.. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE2-0205ARX Biocompatible, Antimicrobial HDPE A biocompatible fractional melt High Density Polyethylene for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided .. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 90HR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Battery Case, Light CoverCAS No. 9003-54-7Information provided by LG Chemical |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 2.0 g/10 min @Load 1.20 kg, Temperature 230 °C |
2.0 g/10 min @Load 2.65 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Luriblend® HIPS E SL5 Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant (5%)Appearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borcoat™ HE3453 Natural High Density Polyethylene for Steel Pipe Coating Borcoat HE3453 is a natural and colorable high density polyethylene produced with the Borstar technology in similar conditions as the black ready made top coat Borcoat HE3450. Borcoat HE3453 is rec.. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total HDPE 6420 High Density Polyethylene, Film Resin Polyethylene: Medium molecular weight, high density film resinCharacteristics:Excellent moisture barrier propertiesLow gelsLow taste and odorHigh stiffnessGood processabilityGood compatibility with.. |
|||
Melt Flow | 2.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 2.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTALUX 9202 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information.. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 100STE NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100STE NC010 (formerly DE20590) is a high-viscosity super-toughened acetal homopolymer with very low VOC emissions. P.. |
|||
Melt Flow | 2.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Denka MALECCA K-400 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3300 Description: General Purpose Utility BlackInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3501 Natural 1050 Description: Natural, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3502 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
Procedure A; ASTM D1238 |
Diamond Polymers ABS TX-541 Description: Super High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg, Temperature 220 °C |
2.0 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXG154 PC (Europe-Africa-Middle East) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Melt Flow | 2.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Samyang Triel® 5720 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5720 is an extrusion grade.Information provided by Samyang. |
|||
Melt Flow | 2.0 g/10 min @Load 5.00 kg |
2.0 g/10 min @Load 11.0 lb |
ASTM D1238/P |
Borealis Borstar® HE6062 HDPE Black Jacketing Compound Borstar HE6062 is a black, bimodal co-polymer high density polyethylene (HDPE) compound produced using the Borealis Borstar process. It is characterized by balanced properties important in jacketin.. |