Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12.1 g/10 min @Load 10.0 kg, Temperature 230 °C |
12.1 g/10 min @Load 22.0 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 10.5 cm<sup>3</sup>/10min.; ISO 1133 |
DSM Arnitel® EB464 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |