Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Melt Flow | 1.4 g/10 min @Load 5.00 kg |
1.4 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total Finathene® 6002 HDPE, blow molding, pipe
(discontinued **) FINATHENE® 6002 is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® 6002 has been especially developed for the manufacturing of toys and of b.. |
|||
Melt Flow | 1.4 g/10 min @Load 5.00 kg |
1.4 g/10 min @Load 11.0 lb |
ISO 1133 |
Total Lacqtene® 2005 TN 59 HDPE pipe
(discontinued **) LACQTENE® 2005 TN 59 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2005 TN 59 is best processed between 190 and 230°C.Informa.. |
|||
Melt Flow | 1.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3003MC Black 1722 Description: BlackInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S610 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA S710 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DSM Arnitel® EB464 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 and ISO 1133 |
ExxonMobil Exxelor™ PE 1040 High Density Polyethylene Resin Product Description: Exxelor PE 1040 polymer resin is a maleic anhydride functionalized high density polyethylene, produced by reactive extrusion. It has been primarily designed to act as a coupli.. |