Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.0 - 7.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 7.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
±15% |
Kazanorgsintez PE2NT21-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Melt Flow | 5.0 - 7.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.0 - 7.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Kazanorgsintez PE2NT 11-9 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended to be processed into pressure p.. |