Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 80 g/10 min @Load 10.0 kg, Temperature 220 °C |
80 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® G151 ABS (Europe-Africa-Middle East) CYCOLAC G151 is a flame retardant grade of ´new technology´ CYCOLAC which has been especially formulated to minimise many of the problems often associated with the processing of traditiona.. |
|||
Melt Flow | 80 g/10 min @Load 10.0 kg, Temperature 220 °C |
80 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East) CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 80 g/10 min @Load 10.0 kg, Temperature 220 °C |
80 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East) CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 80 - 245 g/10 min @Load 21.6 kg, Temperature 190 °C |
80 - 245 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Kazanorgsintez PE2NT21-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Melt Flow | 80 g/10 min @Load 10.0 kg, Temperature 220 °C |
80 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical HIPS 501S PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi.. |
|||
Melt Flow | 80 g/10 min @Load 5.00 kg, Temperature 265 °C |
80 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Melt Flow | 80 g/10 min @Load 2.16 kg, Temperature 160 °C |
80 g/10 min @Load 4.76 lb, Temperature 320 °F |
ASTM D1238 |
Lubrizol Estane® UB450 Thermoplastic Polyurethane Type: Estane® UB450 is a Shore A, polyester based, solvent-borne adhesive thermoplastic polyurethane (TPU).Uses: Solvent Coating.Available in AsiaInformation Provided by The Lubrizol Corporation |