Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MM 74 U High Density Polyethylene - Injection Molding Eraclene MM 74 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution. The polym.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 275 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |
|||
Melt Flow | 4.5 - 7.2 g/10 min @Load 21.6 kg, Temperature 190 °C |
4.5 - 7.2 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.5 - 7.2 g/10 min @Load 21.6 kg, Temperature 190 °C |
4.5 - 7.2 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MM 74 High Density Polyethylene - Injection Molding Eraclene MM 74 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 74 is characterized by a good balance between rigidity and impact.. |
|||
Melt Flow | 4.5 - 7.2 g/10 min @Load 21.6 kg, Temperature 190 °C |
4.5 - 7.2 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6949C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kingfa HF-626 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowHigh impact resistanceApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM-D1238 |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS NAT Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Styron EMERGEâ„¢ 7100 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7100 advanced resin exhibits a balance of properties between impact strength, heat resistance and processability. Its superior natural base color and lot-to-lot color .. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS LE BK Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can .. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 260 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 500 °F |
ISO 1133 |
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can .. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis HC101BF Polypropylene Homopolymer HC101BF is a polypropylene homopolymer. Applications: HC101BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, packa.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
ExxonMobil Exact™ 9371 Ethylene-based Plastomer Resin Product Description: Exact 9371 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Exact™ 9371 Ethylene-based Plastomer Resin Product Description: Exact 9371 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Chi Mei Kibiton® PB-575 SBC Shoe sole industrial accessory |
|||
Melt Flow | 4.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO-1133 |
Chi Mei Polylac® PA-709S ABS - Extrusion Super Impact Extrusion |
|||
Melt Flow | 4.5 g/10 min @Load 10.0 kg, Temperature 250 °C |
4.5 g/10 min @Load 22.0 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® BM6574 BK316 TPC-ET
(Unverified Data**) Hytrel® BM6574 is a 65 nom. Shore D, plasticiser free high performance resin for blow molding and extrusion; it shows ageing resistance up to 150°C, and excellent mechanical properties at elevated.. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 9502 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |