Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 37.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
37.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycolac® INP564 ABS SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Melt Flow | 37.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
37.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® INP564 ABS+SAN SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |