Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers Softflex® 5000 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 3.5 - 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 - 4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4440R (40404) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 3.5 - 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 - 4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4441R (40404) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 3.5 - 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 - 4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6432R (32604) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 3.5 - 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 - 4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6433R (32604) Medium Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 210 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kingfa FW-620 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kingfa HF-618 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kingfa HP-126 Modified ABS Features:UL94 HB @ 1.6-3.0mmHigh impact resistanceHigh flowApplications:LCD cabinetLarge thin-wall partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) I4 HD 7255 High Density Polyethylene HD7255 is a HDPE grade with high impact strength and low warpage.Applications: thick walled, highly stressed transport containers, injection molding.Information provided by Iran Petrochemical Commer.. |
|||
Melt Flow | 3.5 - 5.28 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 - 5.28 g/10 min @Load 4.76 lb, Temperature 374 °F |
±10% |
Kazanorgsintez PE2NT 16-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX7C HF4750K High Density Polyethylene Wire & CableInformation provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133/ASTM D1238 |
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Melt Flow | 3.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ISO 1133 |
Styron Pulse® 920 MG PC/ABS An inherently matt medium heat, medium impact PC/ABS resin, PULSE™ 920 MG is designed for interior automotive applications where a matt aesthetic is required.Information provided by DowThis pro.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-716 ABS - High Flow High flow, medium impact |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 1000 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 1002 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 2512 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3501 GF-10 Description: Reinforced Grade, 10%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.5 - 6.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 - 6.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3501 SHF Description: Super High FlowInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high.. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a.. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Diamond Polymers SAN 263 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 3501 HF Description: High FlowInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.5 - 5.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 - 5.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
UNI EN ISO 1133 |
Breplast Bretene SPM Thermoplastic Composite, 70% HD + 30% PP Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |
|||
Melt Flow | 3.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 1100 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 2510 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |