Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.5 - 13.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
10.5 - 13.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4131L (314F4) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 10.5 - 21 g/10 min @Load 21.6 kg, Temperature 190 °C |
10.5 - 21 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio > 70; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6252J (526F2) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® I2220 PC General purpose polycarbonate with melt flow rate of 10.5.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® IR2240 PC UL rated HB. 200 series recommended when V-2 rating required. Nonhalogenated. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for.. |
|||
Melt Flow | 10.5 - 21 g/10 min @Load 21.6 kg, Temperature 190 °C |
10.5 - 21 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio > 70; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4252J (524F2) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 10.5 g/10 min @Load 2.16 kg, Temperature 210 °C |
10.5 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL.. |
|||
Melt Flow | 10.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
10.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Melt Flow | 10.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
10.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers SAN 268 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |