Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.1 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.1 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Topas Advanced Polymers TOPAS® 8007F-400 Cyclic Olefin Copolymer (COC) TOPAS® 8007F-400 is a robust film extrusion grade designed for blending with polyethylene (PE). It is a moderate clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, .. |
|||
Melt Flow | 10.1 g/10 min @Load 10.0 kg, Temperature 220 °C |
10.1 g/10 min @Load 22.0 lb, Temperature 428 °F |
Procedure A; ASTM D1238 |
Diamond Polymers ABS VP-11 ELG Description: Extrusion Grade, Low Gloss, Flame RetardantInformation provided by Diamond Polymers, Inc. |