Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10 g/10 min @Load 5.00 kg, Temperature 265 °C |
10 g/10 min @Load 11.0 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® 945ASR PC Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Asia Pacific) Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXD9945A PC UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas re.. |
|||
Melt Flow | 10 g/10 min @Load 3.80 kg, Temperature 200 °C |
10 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 10 g/10 min @Load 3.80 kg, Temperature 200 °C |
10 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 10 g/10 min @Load 3.80 kg, Temperature 200 °C |
10 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle .. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-M.. |
|||
Melt Flow | 10 g/10 min @Load 10.0 kg, Temperature 230 °C |
10 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM-D1238 |
Ineos ABS Lustran® 720 ABS, Molding Grade Lustran® ABS 720 resin is a black, virgin injection molding grade of ABS (acrylonitrile butadiene styrene). It is supplied as salt-and-pepper pellets with color concentrate 901802 black. Designed.. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 190 °C |
10 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) I2 HB 7250 High Density Polyethylene I2 (HB 7250) is a high density polyethylene with Propylene as comonomer. It is easy flowing, low warpage, less hard and stiff than I1.Applications: household articles, closures/seals, packaging.Info.. |
|||
Melt Flow | >= 10 g/10 min @Load 5.00 kg, Temperature 190 °C |
>= 10 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
MTM Plastics Dipolen® H Recycled HDPE Blend Dipolen® H is a granulated HDPE with other polyolefin blend for use in either extrusion or injection molding. It can be supplied unmodified or treated with additives according to customer specif.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC1000 PC PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC1000R PC PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics PC1003R PC PC1003R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was .. |
|||
Melt Flow | 10 g/10 min @Load 5.00 kg, Temperature 265 °C |
10 g/10 min @Load 11.0 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® MKD-1016 PA, 55% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 10 g/10 min @Load 5.00 kg, Temperature 265 °C |
10 g/10 min @Load 11.0 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 265 °C |
10 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 200 °C |
10 g/10 min @Load 4.76 lb, Temperature 392 °F |
ASTM D1238 |
Lubrizol Estane® UB400 Thermoplastic Polyurethane Type: Estane® UB400 is a Shore 78A, polyester based, hot melt adhesive with excellent low temperature flexibility thermoplastic polyurethane (TPU).Uses: Extrusion, Powder Coating.Available in AsiaI.. |
|||
Melt Flow | 10 g/10 min @Load 10.0 kg, Temperature 230 °C |
10 g/10 min @Load 22.0 lb, Temperature 446 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 10 g/10 min @Load 10.0 kg, Temperature 240 °C |
10 g/10 min @Load 22.0 lb, Temperature 464 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 260 °C |
10 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C6303 PC+ABS LNP* Lubricomp* Cycoloy_C6303 compound is a Wear resistant (5% PTFE), flame retardant PC+ABS. High heat and good hydrolytic stability. UL listing from Japan and Pacific. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 250 °C |
10 g/10 min @Load 4.76 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East) VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load.. |