Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 59.0 - 74.0 cc/m²/day | 3.80 - 4.77 cc/100 in²/day | 77°F / 0% / RH; ASTM D3985 |
Honeywell Capran® Emblem™ 1000 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ 1000 is a 0.40 mil (10 micron) biaxially oriented nylon 5 film with excellent flex crack resistance and superior clarity properties. Applications: packaging appl.. |