Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 250 cc/m²/day @Thickness 0.00100 mm |
16.1 cc/100 in²/day @Thickness 0.0000394 in |
85% RH; ASTM D398 |
Solvay Specialty Polymers Ixan® SGA-1 Polyvinylidene Chloride (PVDC) IXAN® SGA-1 is a self-adhesive coat for use on aluminum, steel and plastic films, metalized or not. This universal grade may also be used as an adhesion primer for laminating or coating on plasti.. |
|||
Oxygen Transmission Rate | 250 cc/m²/day | 16.1 cc/100 in²/day | 23°C/85%r.h.; DIS 15105-1/-2 |
EMS-Grivory Grivory® CA 6 E PA* Product description: Grilon CA 6 E is a non-extracted copolyamide with a low melting point. Grilon CA 6 E characterizes itself through the following properties Very high flexibility and toughnessVer.. |
|||
Oxygen Transmission Rate | 250 cc/m²/day | 16.1 cc/100 in²/day | 25°C, 1.0 µm, 85% RH |
Solvay Specialty Polymers Ixan® SGA-1 Polyvinylidene Chloride (PVDC)
(Unverified Data**) IXAN® SGA-1 is a self-adhesive coat for use on aluminium, steel and plastic films, metallised or not. This universal grade may also be used as an adhesion primer for laminating or coating on plasti.. |