Oxygen Transmission Rate 6.20 - 14.0 cc/m²/day
0.399 - 0.902 cc/100 in²/day
77°F / 0% / RH; ASTM D3985
Honeywell Capran® K Coated Nylon Film  (discontinued **)
Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil..
Oxygen Transmission Rate 6.20 cc/m²/day
0.399 cc/100 in²/day
23°C, 0% RH; ExxonMobil Method
ExxonMobil Bicor® 110 AXT OPP Film
Product Description: Bicor ASB-X is a two side coated, sealable OPP film delivering an advanced level of moisture and oxygen battier protection. This film is designed for use in (unsupported and sur..
Oxygen Transmission Rate 6.20 cc/m²/day
0.399 cc/100 in²/day
23°C, 0% RH; ExxonMobil Method
ExxonMobil Bicor® 85 AXT OPP Film