Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 54.0 - 70.0 cc/m²/day | 3.48 - 4.51 cc/100 in²/day | 77°F / 0% / RH; ASTM D3985 |
Honeywell Capran® Emblem™ 1200M Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ 1200M is a 0.48 mil (12 micron) biaxially oriented nylon 6 film with a polymeric coating which provides enhanced adhesion to a variety of inks, coatings, and adh.. |
|||
Oxygen Transmission Rate | 54.0 cc/m²/day | 3.48 cc/100 in²/day | 65% RH,23°C |
UBE 1024FD-1 Nylon 6 Film Description: T-die cast film of 25µm in thicknessInformation provided by UBE. |
|||
Oxygen Transmission Rate | 54.0 cc/m²/day | 3.48 cc/100 in²/day | 25°C, 1.0 µm, 85% RH; Coating on BOPP |
Solvay Specialty Polymers Diofan® A 050 Polyvinylidene Chloride (PVDC)
(Unverified Data**) DIOFAN® A 050 is a standard grade PVDC latex for coating on various substrates. It is generally used as a topcoat on paper, cardboard and as a coating on plastic films.Additional Information: PROCE.. |