Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 1200 cc/m²/day @Thickness 0.120 mm, Temperature 21.0 °C |
77.3 cc/100 in²/day @Thickness 0.00472 in, Temperature 69.8 °F |
ASTM D3985 |
PolyOne Versaflex™ CL E95 Thermoplastic Elastomer (TPE) Versaflex™ CL E95 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E95 is also formulated without the use of plasticizer.. |
|||
Oxygen Transmission Rate | 1200 cc/m²/day | 77.3 cc/100 in²/day | dry; ASTM D3985 |
BASF Ecovio® C2332 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2332 is our biodegradable film product containing 18% renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic.. |