Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | >= 10000 cc/m²/day | >= 644 cc/100 in²/day | 25°C, 0% RH; 25um; ASTM D1434 |
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a.. |