| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Water Vapor Transmission | 5.00 g/m²/day | 0.322 g/100 in²/day | ASTM F372 |
| Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
| Water Vapor Transmission | 5.00 g/m²/day | 0.322 g/100 in²/day | 38°C, 90% RH; ExxonMobil Method |
| ExxonMobil Bicor® 120 AB-X OPP Film Product Description: Bicor AB-X is a two-side coated, sealable OPP film designed for general use in many applications, including overwrap, horizontal and vertical packaging. This film is suitable as.. |
|||
| Water Vapor Transmission | 5.00 g/m²/day | 0.322 g/100 in²/day | 38°C, 90% RH; ExxonMobil Method |
| ExxonMobil Bicor® 30 ARW OPP Film Product Description: Bicor ARW is a two-side acrylic coated OPP film designed for use in lamination and monoweb applications, especially for paper ream wrap. The acrylic-coated side with the higher .. |
|||
| Water Vapor Transmission | 5.00 g/m²/day | 0.322 g/100 in²/day | 38°C, 90% RH; ExxonMobil Method |
| ExxonMobil Bicor® 120 LTSC OPP Film Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS.. |
|||
| Water Vapor Transmission | 5.00 g/m²/day | 0.322 g/100 in²/day | ASTM F1249 |
| Chevron Phillips MarFlex® 9608XD HDPE Film Grade This HDPE is tailored for applications that require:Very low gel levelsVery "clear" filmExcellent drawdownEnhanced stiffnessExcellent WVTR for a chill cast filmExcellent ProcessibilityTypical Cast F.. |
|||