Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 145 - 295 g/m²/day | 9.34 - 19.0 g/100 in²/day | Average value: 220 g/m²/day Grade Count:4 |
Overview of materials for Nylon 66, Film This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat.. |