Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 9.00 - 9.00 g/m²/day @Temperature 38.0 - 38.0 °C |
0.580 - 0.580 g/100 in²/day @Temperature 100 - 100 °F |
Average value: 9.00 g/m²/day Grade Count:2 |
Overview of materials for Nylon 66, Film This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Water Vapor Transmission | 0.600 - 9.00 g/m²/day | 0.0386 - 0.580 g/100 in²/day | Average value: 6.12 g/m²/day Grade Count:10 |
Overview of materials for Polyvinyl Dichloride (PVDC) Coated Polyester Film This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC) Coated Polyester Film". Each property range of values reported is minimum an.. |