Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 145 g/m²/day | 9.34 g/100 in²/day | ASTM E398-70 |
DuPont™ Dartek® O-401 Nylon 6,6 Oriented Film, 15 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A machine direction oriented nylon type 6,6 film. Many of the properties of nylon 6,6 film are improved upon orientation, but particularly the overall tou.. |
|||
Water Vapor Transmission | 145 - 295 g/m²/day | 9.34 - 19.0 g/100 in²/day | Average value: 220 g/m²/day Grade Count:4 |
Overview of materials for Nylon 66, Film This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Water Vapor Transmission | 145 g/m²/day | 9.34 g/100 in²/day | ASTM E398-70 |
DuPont™ Dartek® UF-410 Nylon 6,6 Oriented Film, 15 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A monoaxially oriented nylon 6,6 film with good "slip" characteristics, which ensure excellent machinability/runnability even at high relative humidity con.. |