Water Vapor Transmission 50.0 g/m²/day
3.22 g/100 in²/day
ASTM 1249
DuPont™ Clysar® LE Polyolefin Shrink Packaging Film, 60 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film with the lowest shrink force available in the Clysar® line. Dupont Clysar® LES is ..
Water Vapor Transmission 50.0 - 200 g/m²/day
3.22 - 12.9 g/100 in²/day
Average value: 126 g/m²/day Grade Count:6
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Water Vapor Transmission 50.0 - 150 g/m²/day
3.22 - 9.66 g/100 in²/day
DIN EN 12086
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Water Vapor Transmission 50.0 g/m²/day
3.22 g/100 in²/day
85% RH
BASF Ultramid® C33 LN 0.025 mm Blown Film PA6/66
Description: Ultramid® C33 LN is a copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film. Its lower melting point than standard PA 6 is advantageous for coextrusion..
Water Vapor Transmission 50.0 g/m²/day

@Temperature 38.0 °C
3.22 g/100 in²/day

@Temperature 100 °F
90% RH; 1 µm
Solvay Specialty Polymers Diofan® P510 Polyvinylidene Chloride (PVDC)  (discontinued **)
DIOFAN® P510 is an one-component latex, water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. Thanks to..
Water Vapor Transmission 50.0 - 200 g/m²/day
3.22 - 12.9 g/100 in²/day
Average value: 126 g/m²/day Grade Count:6