Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F130 PA6 Film Extrusion, Medium Viscosity |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F130-C PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F130-C2 PA6 Medium Viscosity, Film Extrusion, Lubricated |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F130-C3 PA6 Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F130-E1 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F130-E5 PA6 Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F132 PA6 Film Extrusion, High Viscosity |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F132-C1 PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F132-E1 PA6 Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F132-E2 PA6 High Viscosity, Nucleated, Lubricated, Film Extrusion |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F136 PA6 Very High Viscosity, Film Extrusion |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F136-C PA6 Film Extrusion, Very High Viscosity, Lubricated |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F136-C1 PA6 Very High Viscosity, Film Extrusion, Lubricated |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F136-E1 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F136-E2 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F234-C PA6 Film Extrusion, High Viscosity, Lubricated |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., Film; DIS 15106-1/-3 |
DSM Akulon® XP32-E1 PA6 Film Extrusion, Medium Viscosity, Lubricated, Nucleated |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., Film; DIS 15106-1/-3 |
DSM Akulon® XP36-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., film; DIS 15106-1/-3 |
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., Film; DIS 15106-1/-3 |
DSM Akulon® XP32-C1 PA6 Film Extrusion, Medium Viscosity, Lubricated |
|||
Water Vapor Transmission | 35.0 g/m²/day @Temperature 23.0 °C |
2.25 g/100 in²/day @Temperature 73.4 °F |
at 85% r.h., Film; DIS 15106-1/-3 |
DSM Akulon® XP36-E1 PA6 Film Extrusion, Medium Viscosity, Nucleated, Lubricated |
|||
Water Vapor Transmission | 35.0 g/m²/day | 2.25 g/100 in²/day | Average value: 35.0 g/m²/day Grade Count:16 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |