Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 24.8 g/m²/day | 1.60 g/100 in²/day | ASTM D3833 |
3M 8411 Edging and Reinforcing Tape 3M™ Edging and Reinforcing Tape 8411 is a transparent polyester film tape for many permanent edging and reinforcing types of applications.Information provided by 3M |
|||
Water Vapor Transmission | 24.8 g/m²/day | 1.60 g/100 in²/day | ASTM D3833 |
3M 850 Polyester Film Tape 3M™ Polyester Film Tape 850 can generally be used for splicing and applications where chemical resistance and/or clean removal is necessary. The silver backing is a transparent polyester with a thi.. |