Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 9.00 g/m²/day | 0.580 g/100 in²/day | ASTM D1434 |
NOVA Chemicals Sclair® 14G Butene LMDPE Film Resin Film Properties. Features: Low gel, good opacity, easy processability.Applications: Overwrap film.Data provided by the manufacturer. |
|||
Water Vapor Transmission | 9.00 g/m²/day @Temperature 38.0 °C |
0.580 g/100 in²/day @Temperature 100 °F |
90% RH; ASTM F-372 |
DuPont™ Dartek® B-601 Nylon 6,6 Barrier Film, 25 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A strong transparent nylon type 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. Can be pri.. |
|||
Water Vapor Transmission | 9.00 g/m²/day @Temperature 38.0 °C |
0.580 g/100 in²/day @Temperature 100 °F |
90% RH; ASTM F-372 |
DuPont™ Dartek® B-602 Nylon 6,6 Barrier Film, 38 µm Thickness, PVDC Coated
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, transparent nylon 6,6 film which has a PVDC coating applied to one side for enhanced barrier to oxygen, moisture, grease and odor. It is special.. |
|||
Water Vapor Transmission | 9.00 - 9.00 g/m²/day @Temperature 38.0 - 38.0 °C |
0.580 - 0.580 g/100 in²/day @Temperature 100 - 100 °F |
Average value: 9.00 g/m²/day Grade Count:2 |
Overview of materials for Nylon 66, Film This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Film". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Water Vapor Transmission | 9.00 g/m²/day | 0.580 g/100 in²/day | ASTM F372 |
LyondellBasell Petrothene® LP540200 High Density Polyethylene ApplicationsPETROTHENE LP 5402-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good draw-down. LP 5402-0.. |
|||
Water Vapor Transmission | 9.00 g/m²/day | 0.580 g/100 in²/day | |
Teknor Apex Terraloy™ BP 10000A Thermoplastic Starch + LLDPE Notes: Terraloy™ BP-10001A is a Thermoplastic Starch/LLDPE ready-to-process compound that contains up to 30% of TPS renewable content. This compound is for blown film application. Forms: Pellets A.. |
|||
Water Vapor Transmission | 9.00 g/m²/day | 0.580 g/100 in²/day | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® M34 Polyester Film, 50 Gauge (13 µm), PVDC Coated Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o.. |
|||
Water Vapor Transmission | 9.00 g/m²/day | 0.580 g/100 in²/day | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® M34 Polyester Film, 75 Gauge (20 µm), PVDC Coated Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on one side with a PVDC copolymer. The coating is heat sealable, and is an excellent moisture and o.. |
|||
Water Vapor Transmission | 9.00 g/m²/day | 0.580 g/100 in²/day | at 100°F, 90% RH; ASTM F1249-90 |
Dow Saran® 8 Clear Plastic Barrier Film Saran™ 8 is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double wound rolls.Information provi.. |