Polymer Property : Water Vapor Transmission = 0.540 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 8.38 g/m²/day

@Temperature 38.0 °C
0.540 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 60 SLP OPP Film
Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin..