Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.970 g/m²/day | 0.0625 g/100 in²/day | at 100°F, 90% RH; ASTM F1249-90 |
Dow Saran® 540 Clear Plastic Barrier Film Saran™ 540 is a clear biaxially oriented monolayer barrier film, designed for unit packaging and other applications. It is available in 4 gauge.Information provided by Dow |