Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.100 g/m²/day | 0.00644 g/100 in²/day | 100°F (37.8°C) / 100%RH; ASTM F1249 |
Honeywell ACLAR® 22C (5.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Water Vapor Transmission | 0.100 g/m²/day | 0.00644 g/100 in²/day | ASTM D3833 |
3M 425 Aluminum Foil Tape 3M™ Aluminum Foil Tape 425 is a 5 mil nominal dead soft aluminum foil backing combined with a transparent acrylic adhesive.Information provided by 3M |
|||
Water Vapor Transmission | 0.100 g/m²/day | 0.00644 g/100 in²/day | ASTM D3833 |
3M 427 Aluminum Foil Tape 3M™ Aluminum Foil Tape 427 is a 5 mil nominal dead soft aluminum foil backing combined with a transparent acrylic adhesive. 3M aluminum foil tape 427 offers an easy-release liner.Information provid.. |