Physical Properties Metric English Comments
Water Vapor Transmission 9.31 - 12.42 g/m²/day
0.600 - 0.7998 g/100 in²/day
100°F / 100%RH); ASTM F1249
Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film  (discontinued **)
Description: Capran® Emblem™ 1230 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo..
Water Vapor Transmission 9.31 - 12.42 g/m²/day
0.600 - 0.7998 g/100 in²/day
100°F / 100%RH); ASTM F1249
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film  (discontinued **)
Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many ..
Water Vapor Transmission 9.31 - 12.42 g/m²/day
0.600 - 0.7998 g/100 in²/day
100°F / 100%RH); ASTM F1249
Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film  (discontinued **)
Description: Capran® Emblem™ 2530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo..
Water Vapor Transmission 9.31 g/m²/day
0.600 g/100 in²/day
100°F; E 96/66
Total 6410 HDPE Film Resin
Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw..
Water Vapor Transmission 9.31 g/m²/day

@Temperature 38.0 °C
0.600 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249
DuPont Teijin Films Mylar® CL Polyester Film, 50 Gauge
Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin..