Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 8000 g/m²/day | 515 g/100 in²/day | 38%, 90%RH; DIN 53.122 |
Lubrizol Advanced Materials PEARLTHANE® 18VT80 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 18VT80 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and superior hydrolysis and microbe resistan.. |